Table 4 Within group comparison of initial and final surface roughness values (n = 10)

From: In vitro comparative effects of alcohol-containing and alcohol-free mouthwashes on surface roughness of bulk-fill composite resins

Group

Mean

Std. deviation

t

P value

X-tra fil in water

0.082

0.306

-0.850

0.2851

X-tra fil in alcohol-free Listerine

0.092

0.491

-0.594

0.5672

X-tra fil in alcohol-containing Listerine

0.135

0.329

-1.299

0.2262

Tetric N-Ceram in water

0.0705

0.191

-1.165

0.2742

Tetric N-Ceram in alcohol-free Listerine

-0.007

0.486

0.048

0.9632

Tetric N-Ceram in alcohol-containing Listerine

0.118

0.349

-1.075

0.3102