Skip to main content

Table 2 Comparison of initial and final surface roughness of XTF and N-Ceram composites

From: In vitro comparative effects of alcohol-containing and alcohol-free mouthwashes on surface roughness of bulk-fill composite resins

 

Composite type

Quantity

Std. Deviation

t

P Value

Initial Surface Roughness

X-tra fil

30

0.497

-0.517

0.605

Tetric N-Ceram

30

0.487

Final Surface Roughness

X-tra fil

30

0.601

0.574

0.569

Tetric N-Ceram

30

0.548