Skip to main content

Table 2 Multiple comparisons (Tukey test) show the difference between each two groups in all durations to measure newly formed bone density

From: Comparing the effect of using calcified autogenous nano dentin particles versus micro dentin particles in the healing of mandibular bony defects in New Zealand rabbits

Bone density within the groups TUKEY TEST

durations

G1 vs. G2

G1 vs. G3

G2 vs. G3

After two weeks

0.002*

0.000***

0.012**

After4 weeks

0.087

0.000***

0.015**

After 8 weeks

0.117

0.000***

0.047*