Table 1 Analyses newly formed bone density measurement through different durations in all groups

From: Comparing the effect of using calcified autogenous nano dentin particles versus micro dentin particles in the healing of mandibular bony defects in New Zealand rabbits

Bone density in Hounsfield Unit scores

Duration

Group I (control)

Group II

(Micro dentin P.)

Group III

(Nano dentin P.)

F

P-value

After two weeks

22.5 ± 9.09

47.66 ± 10.74

68.33 ± 12.27

27.186

0.000***

After 4 weeks

100 ± 29.25

209.66 ± 86.39

363.33 ± 110.75

15.298

0.000***

After 8 weeks

468.33 ± 134.56

815 ± 119.07

1241.66 ± 454.33

11.31446

0.001**

  1. There is a highly significant at P-value < 0.001 (**), and extremely significant at P-value < 0.0001 (***)