Table 3 Composition of residue obtained after leaching of liquation-feeding furnace dross in oxalic acid (SQX analysis, 80 °C, 2 h, L:S 10:1, 12.5% wt. H2C2O4)

From: Leaching of liquation-feeding furnace dross as a first step for germanium recovery

Element

O

Zn

C

Pb

Al

Cu

Sn

Ge

Si

Content [% wt.]

43.8

38.6

12.6

1.57

1.25

0.89

0.87

0.15

0.08